Claims for manufacturing process of silane tanned leather for chrome-free ecological silica gel-tannin extract combined with tanned vegetable tanned leather
- Categories:Silane-tanned leather manufacturing process ZL201710723148.1
- Author:
- Origin:
- Time of issue:2021-11-11 11:08
- Views:
(Summary description)
Claims for manufacturing process of silane tanned leather for chrome-free ecological silica gel-tannin extract combined with tanned vegetable tanned leather
(Summary description)
- Categories:Silane-tanned leather manufacturing process ZL201710723148.1
- Author:
- Origin:
- Time of issue:2021-11-11 11:08
- Views:
Information
Claims for manufacturing process of silane tanned leather for chrome-free ecological silica gel-tannin extract combined with tanned vegetable tanned leather
1. A silane tanning leather manufacturing process for chrome-free ecological silica gel-tannin extract combined with tanned vegetable tanned leather, including fur silane soaking, Hydrogen peroxide pre-liming (elimination of sulfide alkali), silane-hydrogen peroxide main deashing (elimination of sulfide alkali), cationic silica gel pretreatment, salt soaking, acid soaking, primary tanning of silicone/silica gel-tannin extract combined primary tanning, cationic silica gel softening , Anionic silica gel-tannin extract dyeing, retanning, filling, fatliquoring, cationic silica gel fixation and mildew-proof treatment, characterized in that:
(1) The step of immersing fur silane in water is as follows: weigh 100 parts of fur by weight in a drum, wash with water for 10 minutes, add 100-150 parts of normal temperature water, 0.1-1 part of KT1717, 0.05-0.3 part of KT3007, and non-ionic degreasing. 0.2-0.5 part of sterilant, 0.1-0.3 part of bactericide, 0.3-1 part of soda ash, 0.1-0.3 part of sodium sulfide, after slow rotation for 3 hours, turn for 30 minutes/stop for 30 minutes, turn and stop for 8-10 hours, the drum , remove the meat, and enter the silicone-coated ash to push the hair;
(2) The step of liming with silica gel is: weighing 5000 parts of water, 30-60 parts of KT1717, 15-40 parts of KT3007, 20-40 parts of liming aid, 30-60 parts of non-ionic degreasing agent, 60-100 parts of sodium hydrosulfide, 240-280 parts of sodium sulfide; stir well, then slowly add 3,000-4,000 parts of lime, and stir while adding to obtain a mortar-packed mortar, apply the mortar-packed mortar on the rabbit skin and meat surface, and the amount of smear on the back line is appropriate Increase, the flesh overlaps, stacking for 6-12 hours, pushing the hair, entering the drum, entering the silane-sulfide alkali to destroy the hair and liming;
(3) The silane-sulfide alkali liming step is as follows: adding 10-30 parts of normal temperature water, 0.1-0.3 parts of KT1717, 0.3-0.5 parts of non-ionic degreasing agent, 0.3-0.5 parts of liming auxiliary, hydrosulfurization 0.5-0.8 part of sodium, 0.5-0.8 part of sodium sulfide, after slow rotation for 1 hour, turn for 30 minutes/stop for 30 minutes, and stop for 2-4 hours; add 0.5-1 part of KT1717, 0.5-1.5 part of alkali sulfide, lime 1-3 parts, turn for 30 minutes / stop for 30 minutes, turn and stop for 2-4 hours; add 0.5-1 part of KT1717, 0.5-1.5 parts of alkali sulfide, 1-3 parts of lime, turn 30 minutes / stop for 30 minutes, turn and stop 2-12 hours; check the damaged hair, after the damaged hair is clean, add 1-5 parts of KT1717, turn it for 2-4 hours, add 30-50 parts of room temperature water, 1-2 parts of lime, and 0.1-0.3 parts of liming aid , turn for 30 minutes/stop for 30 minutes, turn and stop for 2-4 hours; then add 50-80 parts of room temperature water, 1-2 parts of lime, 0.1-0.3 parts of liming aid, turn 30 minutes/stop for 30 minutes, turn off After 2-4 hours, turn on for 5 minutes/stop for 55 minutes, turn on and off for 10-24 hours, and the drum sheet is released. The waste liquid can be used as liming liquid or re-liming liquid for recycling, and then enters into silica gel for re-liming;
(4) The silica gel reliming step is as follows: Weigh 100 parts of caustic soda peels by weight into the drum, add 100-200 parts of liming waste liquid, add 1-2 parts of KT1717, and 0.3 part of non-ionic degreasing agent -0.5 part, lime 3-5 parts, slow speed for 30 minutes/stop for 30 minutes, stop for 4-12 hours; the waste liquid can be used as liming solution or re-liming solution for recycling, wash the lime skin with water and enter the silane - Hydrogen peroxide pre-deashing (elimination of alkali sulfide);
(5) The steps of the silane-hydrogen peroxide pre-deliming (elimination of alkali sulfide) are: adding 50-100 parts of normal temperature water, 1-2 parts of KT1717, 0.3-0.5 part of non-ionic degreasing agent, rotating at a slow speed for 2 hours; adding sulfuric acid 3-5 parts of ammonium, 0.5-1 part of deliming agent, rotate at slow speed for 2 hours; add 1-2 parts of hydrogen peroxide, rotate at slow speed for 4 hours, wash with water, and enter silane-hydrogen peroxide for main deashing (elimination of alkali sulfide);
(6) The silane-hydrogen peroxide main deashing (elimination of alkali sulfide) steps are: adding 30-50 parts of normal temperature water, 2-4 parts of KT1717, 0.3-0.5 parts of non-ionic degreasing agent, rotating at a slow speed for 2 hours; adding sulfuric acid 5-8 parts of ammonium, 0.5-1 part of deliming agent, rotate at slow speed for 2 hours; add 1-2 parts of hydrogen peroxide, rotate at slow speed for 4 hours, rotate at slow speed for 30 minutes/stop for 30 minutes, and stop for 4-12 hours; After washing with water to pH 6.5-7.5, enter into cationic silica gel pretreatment;
(7) The pretreatment steps of the cationic silica gel are as follows: add 30-50 parts of 35 ℃ hot water, 3-5 parts of KT1717, 3-5 parts of KT4031, rotate at a slow speed for 3 hours, and enter the salt immersion;
(8) The salt soaking step is as follows: adding 8-10 parts of industrial salt, 8-10 parts of Yuanming powder, rotating at a slow speed of 3-8 hours at 35°C, and entering the acid soaking;
(9) The pickling step is as follows: adding 0.5-1.5 part of industrial formic acid, adjusting the pH range to 2.5-3, rotating at a slow speed for 8-12 hours, and entering into the primary tanning of silicon aldehyde/silica gel-tannin extract combination;
(10) The silicone aldehyde primary tanning/silica gel-tannin extract combined primary tanning step is: adding 3-5 parts of KT2811, 0.1-0.3 parts of acid-resistant oil, 2-4 parts of KT2034, and rotating at a slow speed for 4-8 hours; adding tannin extract 8-16 parts of glue, 2-4 parts of acid-resistant oil, 4-6 parts of KT2034, 2-4 parts of KT5901, rotate slowly for 8-12 hours; add 1-2 parts of acid-resistant oil, 2-4 parts of KT2034, adjust the temperature to 45°C, rotate at a slow speed for 8-12 hours; leave the drum for 48 hours, squeeze water, shave evenly, and enter into cationic silica gel to soften;
(11) The steps of softening the cationic silica gel are as follows: weigh 100 parts by weight of the shaved and primary tanned leather in a drum, wash twice with water, and adjust the temperature to 45°C; add 100-150 parts of water at 45°C, KT4031 5-8 parts, KT1717 5-8 parts, KT2811 1-3 parts, turn at medium speed for 4-6 hours, add 1-2 parts of baking soda, turn at medium speed for 4-6 hours, enter into anionic silica gel-tannin extract dyeing and retanning ;
(12) The anionic silica gel-tannin extract dyeing and retanning steps are: adding X parts of dye, 3-5 parts of tannin extract, 2-4 parts of KT5901, 6-8 parts of KT2034, 4-6 parts of KT2351, acid-resistant oil in the same bath 3-5 parts, 5-8 parts of general grease, rotate at medium speed at 45°C for 8-12 hours, enter cationic silica gel for fixation and anti-mildew treatment;
(13) The cationic silica gel fixation and antifungal treatment steps are: adding formic acid in the same bath to adjust the pH to 3-3.5, rotating at a medium speed at 45°C for 1 hour, adding 1-3 parts of KT4031 and 0.3-0.5 parts of antifungal agent, Rotate at a medium speed at 45°C for 2 hours, wash with water twice, drum out, and enter into drying and finishing to obtain a leather blank.
2. The water-saving and emission-reducing silane tanned leather manufacturing process of the eco-type silica gel-tannin extract combined tanning skin-friendly eco-flexible vegetable tanned leather according to claim 1, it is characterized in that: described KT1717 is softening replacement and neutralizing silane, KT1717 is a weak cationic emulsion polymerized side-polyaminohydrocarbyl polyhydroxyhydrocarbyl triethoxysilane hydrocarbyl polymethylsilsesquioxane water emulsion, also known as: water-soluble organosilicon polymer silane coupling agent, low-temperature coupling self-crossing agent Hydroxy-hydrocarbyl silicone oil, technical specifications: 20℃ density 0.95 g/ml, water-soluble content 20±1%, solvent water, pH value 6.5±0.2, viscosity 40-50 mPa.s, appearance is light blue lotion.
3. The water-saving and emission-reducing silane tanning leather manufacturing process of ecologically-type silica gel-tannin extract combined tanning skin-friendly eco-flexible vegetable tanned leather according to claim 1, is characterized in that: described KT3007 is a permeable cross-linked silane auxiliary agent, KT3007 is an isopropanol aqueous solution of a polyepoxy alcohol ether hydrocarbyl polymethylsiloxane silane coupling agent. The technical specifications are: 20 ℃ density 0.85g/ml, non-volatile component weight percentage 36±1%, solvent water, PH The value is 6.5±0.2, the charge is non-ionic, the viscosity is 90-110mPa.s, and the appearance is light yellow to colorless transparent liquid.
4. The water-saving and emission-reducing silane tanned leather manufacturing process of ecologically-type silica gel-tannin extract combined tanning skin-friendly ecological flexible vegetable tanned leather according to claim 1, it is characterized in that: described KT4031 is cationic polyurethane retanning silica gel, KT4031 It is a water-soluble cationic polyurethane polymer silane coupling agent with coupling and cross-linking activity, and is also a strong cationic polyalkoxysiloxane urethane-grease-silica gel polymer; technical index: 20 ℃ Density 0.95 g/ml-1.05g/ml, water-soluble content 18-22%, solvent water, pH value 4.5±0.3, viscosity 400-500 mPa.s, appearance is milky yellow emulsion.
5. The water-saving and emission-reducing silane tanned leather manufacturing process of ecological type silica gel-tannin extract combined tanning skin-friendly ecological flexible vegetable tanned leather according to claim 1, is characterized in that: described KT2811 is aminosilane-modified fatty aldehyde, KT2811 is a water-soluble silicone polyvinylpolyamine basic polymer silane coupling agent, which has good cross-linking and hybridization modification, penetration and dispersion. The technical indicators are: PH value 2-4, weak cationic charge Appearance is light blue emulsion.
6. The water-saving and emission-reducing silane tanned leather manufacturing process of eco-type silica gel-tannin extract combined with tanning skin-friendly eco-flexible vegetable tanned leather according to claim 1, is characterized in that: described KT2034 is a foamy sensual filling silica gel, KT2034 It is a secondary derivative of lecithin and hydroxyalkylaminohydrocarbylcarboxyalkylpolyalkoxysilyl modified polymethylsiloxane. The technical indicators are: 20℃ density 0.92 g/ml, water-soluble content 26-30%, solvent Water, pH value 3.8±0.2, viscosity 150-180mPa.s, appearance is light milky yellow thick liquid.
7. The water-saving and emission-reducing silane tanning leather manufacturing process of ecological type silica gel-tannin extract combined tanning skin-friendly ecological flexible vegetable tanned leather according to claim 1, it is characterized in that: described KT5901 is silicon sulfone filling synthetic tanning agent, KT5901 is a secondary hydrolysis and condensation polymer tanning agent of naphthol sulfonic acid and SO2 organic derivatives with high-quality filling performance of silicon sulfone bridged structure. Content 46%-50%, solvent water, pH value: 4.0±0.2, viscosity: 120mPa·S-140mPa·S, appearance is light brown translucent thick liquid.
8. The water-saving and emission-reducing silane tanned leather manufacturing process of eco-type silica gel-tannin extract combined tanning skin-friendly ecological flexible vegetable tanned leather according to claim 1, is characterized in that: described KT2351 is foaming elastic fatliquoring silicone oil, KT2351 is a modified polymeric silicone oil, a water-emulsion copolymer of modified reactive silicone oil and vinylamino and carboxyl monomers. The content is 28-33%, solvent water, pH value 4.5-5.5, viscosity 24000-26000 mPa.s, appearance is milky yellow thick liquid.
9. The water-saving and emission-reducing silane tanned leather manufacturing process of eco-type silica gel-tannin extract combined tanning skin-friendly ecological flexible vegetable tanned leather according to claim 1, is characterized in that: KT1717, KT3007, KT2811, KT4031, KT2034, KT5901 , KT2351 and other industrial products were purchased from Minnida Silicon Fluoride Application Research and Pilot Plant in Wenjiang District, Chengdu.
Scan the QR code to read on your phone
Next:
Patent certificate 481